※ 以150 nm及以下帶寬的Ti寶石激光器應用做產(chǎn)品說明
一、激光反射鏡:
139691鍍膜,HRs,p(0 – 10°, 725 – 875 nm) > 99.9 %,| GDD-Rs,p(0–10°, 725 – 875 nm) | < 50 fs2
140876鍍膜,HRs,p(0 – 10°, 750 – 850 nm) > 99.5%,| GDD-Rs,p(0 – 10°, 750 – 850 nm) | < 60 fs2,高功率應用

139943鍍膜,HRs,p (0 – 45°, 725 – 875 nm) > 98 %,| GDD-Rs,p (45°, 725 – 875 nm) | < 40 fs2

二、泵浦端鏡:S2面140872鍍膜, HRs,p (0 – 10°, 725 – 875 nm) > 99.9 %,Rs,p (0 – 10°, 500 – 545 nm) < 2 % S1面鍍膜 140875,ARs,p (0 – 10°, 500 – 545 nm) < 0.2 %

三、轉(zhuǎn)向鏡:
139710鍍膜,HRs,p (22.5°, 725 – 875 nm) > 99.9 %,| GDD-Rs,p (22.5°, 725 – 875 nm) | < 75 fs2

139693鍍膜,HRs,p (45°, 740 – 860 nm) > 99.9 %,| GDD-Rs,p (45°, 740 – 860 nm) | < 75 fs2

139711鍍膜,HRp(45°, 725 – 875 nm) > 99.8 %,GDD-Rp (45°, 725 – 875 nm) = -40 (±30) fs2

140881鍍膜,HRs (45°, 730 – 870 nm) > 99.8 %,HRp (45°, 760 – 840 nm) > 99.5 %,| GDD-Rs,p (45°, 760 – 840 nm) | < 80 fs2,高功率應用

四、分光鏡
750-850/360-450 nm:S2面160927鍍膜,HR (0°, 750 – 850 nm) > 99.9 %,R (0°, 360 – 440 nm) < 5 %, | GDD-R (0°, 750 – 850 nm) | < 40 fs2;S1面160929鍍膜,AR (0°, 360 – 440 nm) < 0.5 %

760-850/350-450 nm:S2面113728鍍膜,HRu (45°, (760 – 850 nm) ±5 nm) > 99.9 %, Ru (45°, (360 – 440 nm) ±5 nm) < 2 %,| GDD-Ru (45°, 760 – 850 nm) | < 40 fs2,| GDD-Tu (45°, 360 – 440 nm)| < 40 fs2; S1面124879鍍膜,AR (45°, 350 – 450 nm) < 0.7 %

五、啁啾鏡(對):
140884鍍膜,HRs,p (0 – 10°, 725 – 875 nm) > 99.9 %,GDD-Rs,p (0 – 10°, 725 – 875 nm) = -40 (±10) fs2

140988+140990鍍膜,HRs,p (0 – 10°, 725 – 875 nm) > 99.8 %,GDD-Rs,p (0 – 10°, 725 – 875 nm) = - 40 (±20) fs2

141560+141561鍍膜,HRs,p (0 – 10°, 725 – 875 nm) > 99.9 %,GDD-Rs,p (0 – 10°, 725 – 875 nm) = -80 (±40) fs2

141570+141571鍍膜,HRs,p (0 – 10°, 725 – 875 nm) > 99.8 %,GDD-Rs,p (0 – 10°, 725 – 875 nm) = -110 (±50) fs2

六、分束鏡
s偏振:S2面141113鍍膜,PRs (45°, 725 – 875 nm) = 50 (±2) %,| GDD-Rs (725 – 875 nm) | < 5 fs2; S1面141114鍍膜,ARs (45°, 725 – 875 nm) < 0.5 %

p偏振:S2面141122鍍膜,PRp (45°, 725 – 875 nm) = 50 (±2) %,| GDD-Rp (725 – 875 nm) | < 20 fs2; S1面141121鍍膜,ARp (45°, 725 – 875 nm) < 0.2 %

七、窗口:S2+S1鍍膜140890,ARs,p (0 – 15°, 725 – 875 nm) < 0.2 %

|